I went down to the workshop at 0200 tonight (I like to stay up late, but get really tired the next day) to check on our laminating work. I am really happy that I did. Two massive airbubbles/areas where the glass had pulled off. Both about 10cm long and 4cm wide. This was two hours after we finished laminating, so the epoxy had not hardened yet. Some quick work with a squeege and it looked good again. This morning the epoxy had hardened substantially and it looked good.
Going over the lamniate again after some hours have become routine when not using the vacuum pump. Usually I find some small air bubbles to remove and stuff like that.